Set-Top Box IR Window: What Dark Plastic Does at 15 kV Air
A set-top box loses remote control range after a ±15 kV air discharge to the dark window in front of the IR receiver. The receiver still responds at one metre but not at four. The window is a 1.5 mm carbon loaded plastic with a surface resistivity near 10¹² ohm per square, and its inner face sits 6 mm from the receiver lens.
Direct answer
At 15 kV the window is not an insulator. The carbon fill brings surface resistivity down to 10¹² ohm per square, so charge spreads across the window and creeps the 6 mm to the receiver shield, coupling into the automatic gain control node. Either raise surface resistivity above 10¹⁴ or wrap the aperture with a grounded frame that collects the charge before it reaches the lens, and keep a 5 V low capacitance part on the receiver output so the AGC node cannot be pulled far enough to collapse the gain.
Four paths into one receiver
| Path | What it is | Normal state | Part needed | Why |
|---|---|---|---|---|
| Window outer surface | Carbon loaded plastic, 1.5 mm | Floating | No part, raise resistivity | Charge spreads before it arcs |
| Window inner face to shield | 6 mm creepage | 0 V at the shield | No part, grounded frame | Creepage is the actual entry |
| Receiver output | 38 kHz demodulated, 3.3 V logic | 0 or 3.3 V | Yes, ESD3V3D500TA | The AGC node sits behind it |
| Receiver supply | 5 V, 3 mA | 5 V | Yes, ESD5D150TA | A dip resets the gain loop |
| Front panel ground | Paint to chassis | 0 V | No part, bare contact | Paint thickness sets the bond |
Creepage, not breakdown, decides
The 1.5 mm wall of the window would hold about 4.5 kV if the material were a clean insulator, and 15 kV would still cross it. What actually happens first is surface creep: with 10¹² ohm per square, a 15 kV charge spreads over a few square centimetre and the 6 mm band between the window edge and the shield sees about 2.5 kV/mm, which is below the 3 kV/mm air figure but well above what a contaminated surface holds. Fingerprint grease drops the surface resistivity by two orders of magnitude, which is why the failure appears on units that have been in use for months and never on a clean sample in the lab.
Three trade-offs behind the window
First, darkness and conductivity come from the same dye. Carbon black gives the near infrared transparency the receiver needs and the dark look the industrial design asks for, and it also sets the surface resistivity. A dyed resin without carbon keeps resistivity above 10¹⁴ and costs nothing in optical performance, so ask the moulder which route was used. Second, the frame beats the coating. A grounded metal frame around the aperture collects the creepage current at the edge and is stable over life; a conductive coating on the window wears at the finger contact area. Third, the part goes on the output, not the lens. A part across the photodiode adds capacitance to a high impedance node and slows the 38 kHz envelope.
Four steps that separate material from layout
Measure surface resistivity on a used window, not a new one, with a concentric ring probe at 500 V and 50 percent relative humidity. Discharge the window centre at ±15 kV air, 10 times, and record the remote range at which the box still responds. Repeat with the aperture frame grounded and compare the range. Finally check the receiver output with a scope while a 38 kHz burst arrives, looking for a gain collapse that lasts longer than 100 ms, because a shorter dip is recovered by the next frame and never shows up as a field complaint.
FAQ
Can a clear window with a black bezel solve it?
Yes, and it is the cleaner route. A clear infrared transparent resin keeps surface resistivity above 10¹⁴, and the black look comes from the bezel moulding behind it. The receiver sees the same optical signal and the creepage path disappears.
Why does the remote work up close but fail at four metres?
A collapse of the AGC gain reduces sensitivity by 20 dB or more. A remote at one metre still delivers enough optical power to trip the comparator, while the same remote at four metres delivers roughly one sixteenth of that power and falls below the reduced threshold.
Sources
Source check date: 2026-11-06. Surface resistivity and creepage figures are from one production sample measured at 50 percent relative humidity; values shift with contamination and with moulding batch.
Related News
2025.02.24
Selection knowledge of ESD static diodes and TVS tubes
2026.06.13
ESD Protection for Industrial Communication Buses: RS-485, CAN, Modbus, and Profibus Complete Guide
2026.07.20
For which automotive applications is the SM8S series TVS suitable?
2026.07.24
How to Choose Between Unidirectional and Bidirectional TVS: A Comparison of DC Power Supplies, AC Signals, and Communication Interfaces
2026.07.28
How to remediate EMC radiated emission failures? Troubleshooting clocks, cables, and PCB return paths.
2026.08.06
How to Read ESD Diode Capacitance for High-Speed Interfaces